20cr硬度較高,韌性比15CrA差,該鋼具有比較好的淬透性、中等的強度和韌性。油淬到半馬氏體硬度的淬透性為Φ20-Φ23mm。該鋼經滲碳淬火表面強化處理后,在模具表面會獲得細針狀回火馬氏體,硬度為58-62HRC;心部獲得低碳馬氏體組織,硬度35-40HRC,基體強韌性高,可滿足冷作模具高硬度、高強度、高韌性和適當的耐腐蝕性的使用性能要求。正火可促進組織球化,細化大塊狀先共析鐵素體,改進毛胚的切削性能。
![](http://m.skatingpune.com/file/upload/sichuanpanlong/202008/30/2037518624134525.jpg)
![u=3183769759,2934323849&fm=26&gp=0](http://m.skatingpune.com/file/upload/sichuanpanlong/202009/07/1130502006254525.jpg)
![](http://m.skatingpune.com/file/upload/sichuanpanlong/202008/30/2037521421918525.jpg)
![](http://m.skatingpune.com/file/upload/sichuanpanlong/202008/30/2037539769883525.jpg)
![](http://m.skatingpune.com/file/upload/sichuanpanlong/202008/30/2037542807575525.jpg)
![](http://m.skatingpune.com/file/upload/sichuanpanlong/202008/30/2037555195835525.jpg)
![](http://m.skatingpune.com/file/upload/sichuanpanlong/202008/30/2037571674234525.jpg)
![](http://m.skatingpune.com/file/upload/sichuanpanlong/202008/30/2037587607459525.jpg)
網站公告 新聞中心
聯系方式
站內搜索 友情鏈接 |
產品參數
詳細信息 ![]() 20cr硬度較高,韌性比15CrA差,該鋼具有比較好的淬透性、中等的強度和韌性。油淬到半馬氏體硬度的淬透性為Φ20-Φ23mm。該鋼經滲碳淬火表面強化處理后,在模具表面會獲得細針狀回火馬氏體,硬度為58-62HRC;心部獲得低碳馬氏體組織,硬度35-40HRC,基體強韌性高,可滿足冷作模具高硬度、高強度、高韌性和適當的耐腐蝕性的使用性能要求。正火可促進組織球化,細化大塊狀先共析鐵素體,改進毛胚的切削性能。 ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() 聯系方式
|